个性化文献订阅>期刊> ADVANCED MATERIALS
 

Tensile Tests on Individual Single-Walled Carbon Nanotubes: Linking Nanotube Strength with Its Defects

  作者 Wang, MS; Golberg, D; Bando, Y  
  选自 期刊  ADVANCED MATERIALS;  卷期  2010年22-36;  页码  4071-4075  
  关联知识点  
 

[摘要]The ultimate tensile strength of individual single-walled carbon nanotubes (CNTs) is measured in a high-resolution transmission electron microscopy equipped with a conducting atomic force microscopy unit. The values are correlated to every tube's structural details. The strength of similar to 100 GPa, approaching the theoretical limit for defect-free CNTs, is documented in tubes without visible defects; for those with spatially separated stepwise pentagon-heptagon defects, determining the breaking sites, it reduces to 40-70 GPa.

 
      被申请数(0)  
 

[全文传递流程]

一般上传文献全文的时限在1个工作日内